Abstract
A novel molecularly imprinted polymer (MIP) coated bulk acoustic wave (BAW) sensor was fabricated for liquid phases. It can be used as a sensitive portable implement for the assay of 2,4-dichlorophenoxyacetic acid. A logarithmic response relationship between 2.0 x 10(-7) M and 5.0 x 10(-4)M was found. The detection limit was 1.0 x 10(-7) M. Recoveries were 93.2-108.7%. Influencing factors were investigated in detail and optimized.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.