Abstract
This study investigates a purification process for metallurgical-grade silicon (MG-Si) in which Si is alloyed with tin (Sn) and CaO–SiO2–CaCl2 slag is used to remove boron (B) impurity. Acid leaching was performed to remove the Sn phase after slag refining to recover high-purity Si from the Si–Sn alloy. The effect of refining time was investigated, and acceptable refining results were realized within 15 min. The effects of slag composition and Sn content on the removal of B were also studied. The results indicate that increasing Sn content favors B removal. With the increase of Sn to 50% of the alloy, the final B content decreased to 1.1 × 10−4wt%, 93.9% removal efficiency.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: International Journal of Minerals, Metallurgy, and Materials
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.