Abstract

The effect of slag treatment with Copper addition in silicon purification by metallurgical methods was examined in this paper. The microstructures and contents of Si-Cu alloy after slag refining were investigated by XRD and ICP, respectively. The majority phases in the Si-Cu alloy were Cu3Si and Si. The partition ratio of boron (LB) between slag and silicon was studied with and without Cu addition. Experimental results show that slag treatment with Cu addition can improve the LBin CaO-SiO2-CaF2slag system, where a maximum boron removal ratio of 85% could be achieved.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.