Abstract

Environmentally benign Bi3.25La0.75Ti3O12 (BLTO) thin film capacitors were prepared by a cost effective chemical solution deposition method for high energy density storage device applications. Low annealing temperature annealed BLTO thin films showed very slim hysteresis loops with high maximum and small remnant polarization values. Increasing the applied electric field to 2040 kV/cm, the optimized BLTO thin films show a high recoverable energy density of 44.7 J/cm3 and an energy efficiency of 78.4% at room temperature. Additionally, the BLTO thin film capacitors exhibited excellent fatigue endurance after 4 × 108 cycles and a good thermal stability up to 140 °C, proving their strong potential for high energy density storage and conversion applications.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.