Abstract
The aim of this study is to estimate the velocity of fatigue crack growth (crack growth rate - CGR) from the texture in SEM images of crack surfaces. A simple and quick method is based on fitting training images as a linear combination of several small subimages selected from the images themselves. The size of basic subimages is derived from autocorrelation functions of the image in row and column direction. The selection of basic subimages is based on two indicators: "appeal" evaluating their shape content, and mutual coefficient of correlation. The method is easy to implement and quick in computations, while results of testing application are fully comparable with best ones obtained within textural fractography of fatigue failures.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.