The photocathodic hydrogen evolution reaction (HER) from p-type Si nanowire (NW) arrays was evaluated using platinum deposited by atomic layer deposition (ALD) as a HER cocatalyst. ALD of Pt on the NW surface led to a highly conformal coating of nanoparticles with sizes ranging from 0.5 to 3 nm, allowing for precise control of the Pt loading in deep submonolayer quantities. The catalytic performance was measured using as little as 1 cycle of Pt ALD, which corresponded to a surface mass loading of ∼10 ng/cm(2). The quantitative exploration of the lower limits of Pt cocatalyst loading reported here, and its application to high-surface-area NW photoelectrodes, establish a general approach for minimizing the cost of precious-metal cocatalysts for efficient and affordable solar-to-fuel applications.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.