Abstract
AbstractThe development of deposition processes for metal carbide thin films is rapidly advancing, driven by their potential for applications including catalysis, batteries, and semiconductor devices. Within this landscape, atomic layer deposition (ALD) offers exceptional conformality, uniformity, and thickness control on spatially complex structures. This paper presents a comprehensive study on the thermal ALD of MoCx with MoCl5 and 1,4‐bis(trimethylgermyl)‐1,4‐dihydropyrazine [(Me3Ge)2DHP] as precursors, focusing on the functional properties and characterization of the films. The depositions are conducted at 200–300 °C and very smooth films with RMS Rq ≈0.3–0.6 nm on Si, TiN, and HfO2 substrates are obtained. The process has a high growth rate of 1.5 Å cycle−1 and the films appear to be continuous already after 5 cycles. The films are conductive even at thicknesses below 5 nm, and films above 18 nm exhibit superconductivity up to 4.4 K. In lieu of suitable references, Raman modes for molybdenum carbides and nitrides are calculated and X‐ray diffraction and X‐ray photoelectron spectroscopy are used for phase analysis.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.