ABSTRACTCerium dioxide (CeO2) thin films were deposited by atomic layer deposition (ALD) on both Si and TiN substrates. The ALD growth produces CeO2 cubic polycrystalline films on both substrates. However, the films show a preferential orientation along <200> crystallographic direction for CeO2/Si or <111> for CeO2/TiN. In correspondence, we measure a relative concentration of Ce3+ equals to 22.0% in CeO2/Si and around 18% in CeO2/TiN, by X-ray photoelectron spectroscopy. Such values indicate the presence of oxygen vacancies in the films. Our results underline the films differences and similarities between ALD-deposited CeO2 either on Si or TiN substrates, thus extending the knowledge on the CeO2 structural and chemical properties.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.