Abstract
Flowchart illustrating how the films are deposited (a) without and (b) with cleaning step, and Auger electron spectroscopy depth profile of 15 nm HfNx deposited with precleaning step, before annealing (c) and after 900 °C annealing at NH3 atmosphere.