Abstract

We explore three variants of atomic layer deposition (ALD) to deposit titanium oxide on the soft polymer polydimethylsiloxane (PDMS). We show that the organic solvent resistance of PDMS is increased by two orders of magnitude compared to uncoated PDMS for ALD performed at atmospheric pressure, which results in a unique surface–subsurface coating of PDMS.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.