Abstract The reversible thermochromic insulator–metal transition (IMT) of VO2 is believed to start from suitable nucleating defects, but the role of specific defects during the IMT has remained elusive. In this work, we performed a simple, mild but effective acid etching treatment on pure-phase VO2 films to adjust the surface state of the VO2 particles while leaving the phase composition, crystallinity, grain size, and stoichiometry unchanged. By continuously etching VO2 particles, the poor crystallized layers on the particle surface were removed, and the particle connections became loose, resulting in significant shifts of the IMT toward higher temperatures. In stark contrast, the reversal IMT (i.e., metal–insulator transition, MIT) parameters remained relatively steady during the etching process. These experimental results correlate directly the IMT characteristics with the states (e.g., local defects, stress, and connection) of the particle surface, and further enable us to asymmetrically modulate the IMT parameters, while keeping the MIT (i.e., metal–insulator transition, the reversal of IMT) almost constant. This work illustrates the potential for particle surface engineering in thermochromic VO2 films.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.