Abstract

In this study, lithium slag was utilised as a supplementary cementitious material (SCM) to develop pozzolanic activity and reduce CO2 emissions related to cement production, with a focus on comprehensive chemical tests and microstructural assessments. Lithium slag was primarily characterised through laser particle size analyser, X-ray fluorescence, X-ray diffraction, scanning transmission electron microscopy coupled with energy dispersive X-ray spectroscopy, and thermogravimetry. These tests indicate that lithium slag holds 31.6% amorphous phase with rich aluminosilicate minerals, making it an excellent candidate as pozzolan. The unsaturated lime and electrical conductivity pozzolanic activity precursor tests evaluated the potentiality of using lithium slag as a low carbon pozzolan. The optimum percentage of lithium slag as a supplementary cementitious material was determined from Frattini, strength activity index, and R3 tests by replacing 0–60% cement. Results show that 40% lithium slag mortar could achieve 93% strength activity index in 28 days. The microstructure development of lithium slag was assessed and ettringite, monocarboaluminate, and intermixed calcium aluminosilicate hydrates were formed at 56 days.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.