AbstractIn this research, five fracture criteria (maximum tangential stress (MTS), generalized maximum tangential stress (GMTS), minimum strain energy density (SED), generalized minimum strain energy density (GSED), and modified maximum tangential stress (MMTS)) were evaluated for asphalt concrete using fracture data from tests conducted under various loading modes and conditions. Tests were performed on semi‐circular bend (SCB) specimens of various sizes. Based on the results, the MTS criterion tends to overestimate fractures, while the GMTS criterion exhibits more precise predictions. The SED and GSED criteria inaccurately predict fractures, especially under certain loading conditions. The MMTS criterion shows superior predictive capability for asphalt concrete fractures. Specimen size influences fracture resistance, with larger specimens exhibiting higher fracture values. Overall, the MMTS criterion closely mirrors the crack growth behavior of asphalt concrete, highlighting its precision in predicting fracture results. The errors between the predictions of the fracture criteria MTS, GMTS, SED, GSED, and MMTS, and the experimental results ranged from 0% to 42.8%, 0% to 22.5%, 0% to 52.7%, 0% to 42.4%, and 0% to 14.5%, respectively.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Fatigue & Fracture of Engineering Materials & Structures
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.