Abstract

The T92 martensitic and Super304H austenitic dissimilar steels welded joints were always encountered in the super critical boilers. The isothermal method was used to assess the creep rupture strength of weld joints. With the higher loading stress, the transcrystalline fracture was the rupture mode of creep specimens, and results in forming dimples. With the higher loading stress, the transcrystalline fracture was the rupture mode of creep specimens and results in forming dimples. With the lower loading stress, creep cavities joined each other along the grain boundary, the creep rupture was the rupture mode of creep specimens and results in cleavage rupture.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.