Abstract

As the problem of shrinkage on wool fabric, the chitosan was applied to solve it in this paper. The volume of retraction bulb and strength were considered to describe the results of anti-shrinkage after the finishing. It shows that great anti-shrinkage is got in this experiment, and the best treatment process is defined as follow: the concentration of chitosan 6g/l, pH 5, 80min, 90°C and bath ratio 1:50.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.