Abstract

Penetration and conversion of adhesives into the hybrid layer (HL) is important to the quality and longevity of the adhesive resin (AR)-dentin bond. In this study, a methodology is developed to examine the degree of conversion and relative HEMA concentration with respect to Bis-GMA using Raman spectroscopy. This methodology will be used in the future reports related to this topic. Conversion in the AR of water-stored resin-dentin samples (84% +/- 3%) agreed well with that measured in commercial adhesive (Comm Adh) resin samples after 24-h water storage (80% +/- 2% from Part 1) and was significantly higher than Comm Adh without water storage (58% +/- 3% from Part 1) (p = 0.0005). Adhesive conversion was not significantly different (p = 0.5036) through the middle of the HL, with a mean of 83% +/- 6%. HEMA mole fraction, relative to Bis-GMA, was significantly higher (p = 0.0028) in the top half of the HL (0.67 +/- 0.03), when compared to HEMA in the AR (0.60 +/- 0.01). HEMA and EDMAB were identified through GC/MS as leachable components in the aqueous 24-h storage media. The effect of this elution explains the change in conversion measurements observed between dry and water-stored conditions, which is more appropriately described as the "apparent" conversion.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.