Abstract
Lattice imperfections were produced in KCl crystals by a thermal process. The heat treated specimen was irradiated with 50 KeV electrons and the corresponding range of electrons in the crystal has been estimated. It was found that the electron range in the crystal depends upon the temperature of heat treatment, being a decreasing function of this temperature up to about 625 K, above which it becomes an increasing function. This anomaly has been explained in terms of dissolution of vacancies through dislocation loops.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.