Abstract

Semiconducting boron doped single-crystal CVD diamond has been patterned using aluminum masks and an inductively coupled plasma (ICP) etch system. For comparison insulating HPHT diamond samples were also patterned using the same process. Diamond etch rates above 200 nm/min were obtained with an O 2/Ar discharge for a gas pressure of 2.5 mTorr using 600 W RF power. We have accomplished the fabrication of structures with a minimum feature size of 1 μm with vertical sidewalls in both CVD and HPHT diamond. The ICP etching produced smooth surfaces with a typical root-mean-square surface roughness of 3 nm. The dependence of etch rate on bias voltage was somewhat different for the two types of diamond. However, for all samples both the etch rate and anisotropy were found to improve with increasing bias voltage.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.