Abstract

AbstractNatural human hair was modified by the graft polymerization of propylene sulfide in an aqueous medium. The amount of the polymer grafted onto the reduced hair was 0.15–0.19 g on 1.0 g of hair. The grafted polymer was isolated by the hydrolysis of the hair in the polymer‐grafted hair under basic conditions and was confirmed to be poly(propylene sulfide) by 1H NMR, 13C NMR, and Fourier transform infrared spectra. The number‐average molecular weights of the isolated polymers from the grafted products were 10,000–12,000. © 2006 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 44: 3778–3786, 2006

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.