In current research, WC dissolution phenomenon happened in TIG welds was investigated and discussed. And the element diffusion was studied using area-scanning method. The results showed that the WC dissolution phenomenon always happened near WC-Co/Welded seam interface. Moreover, the amount of WC dissolved in welds became less from WC-Co, welds to invar alloys. WC dissolution happened in welded seam induced by tungsten arc led to the WC grain growth (60µm or so) and WC shape changes. The grain boundary (GB) between different WC particles during WC aggregation was also confirmed and WC grain growth was owed to the WC aggregation during the processing of WC dissolution.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.