Abstract
Analysis of the results of the microstructure and the mechanical properties change in AA1050 aluminum alloy of technical purity processed using ECAP (Equal Channel Angular Pressing) and KoBo deformation methods are presented in the paper.. ECAP process was performed according to Bc scheme in the range from 1 up to 10 passes. Changes of microstructure were analyzed using scanning electrone microscope equipped with electron backscattered diffraction (EBSD) system. Microstructure and fraction of high-angle grain boundaries in KoBo processed samples were similar to those observed in ECAP processed samples after four passes. The most significant microstructure refinement was observed in ECAP processed sample submitted to 10 passes. In ECAP method the systematic increase of mechanical properties was observed along with increase of deformation degree.