This research “the analysis of different welding speeds, the micro structure on the welded joints of silicon steel pipe” has been carried out on precise and accurate measurements of parameters. The effects of different laser powers on the weld material have critically been studied and analyzed. Welding speeds have great effect on the micro-structure and morphology of the weld material. The determination of the basic components of the active agent is the key of the preparation. The active materials selected in this experiment are the commonly used oxides (SiO2, TiO2, and Cr2O3) and fluoride (NaF) reagents. However, the comprehensive experiment contains a large number of the level of combination; the workload is huge, due to the experimental site, experimental materials, funding, and time constraints lead to low efficiency. In the laser welding of silicon steel sheet, coating active agent can increase the penetration depth and affect the weld formation, and the influence of active agent NaF and SiO2 on weld penetration of silicon steel sheet is significant. The formula G is the most effective in increasing the penetration depth, including 25% SiO2, 25% TiO2, 12.5%Cr2O3 and 37.5% NaF.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.