Abstract
In this paper, a new small-sized (two-bar) specimen type, which is suitable for use in obtaining both uniaxial creep strain and creep rupture life data, is described. The specimen has a simple geometry and can be conveniently machined and loaded (through pin-connections) for testing. Conversion relationships between the applied load and the corresponding uniaxial stress, and between the measured load-line deformations and the corresponding uniaxial minimum creep strain rate, have been obtained, based on the reference stress method (RSM), in conjunction with finite element analyses. Using finite element analyses the effects of the specimen dimensions on reference stress parameters have been investigated. On this basis, specimen dimension ratio ranges are recommended. The effects of friction, between the loading pins and the specimen surfaces, on the specimen failure time, are also investigated. Test results obtained from two-bar specimen tests and from corresponding uniaxial specimen tests, for a P91 steel at 600 °C, are used to validate the test method. These results demonstrated that the specimen type is capable of producing full uniaxial creep strain curves. The advantages of this new, small, creep test specimen, for determining uniaxial creep data, are discussed and recommendations for future research are given.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.