Abstract
Quantitative monitoring of steel corrosion plays a crucial role in evaluating structural safety and predicting structural performance. The electromechanical impedance (EMI) technique has already emerged for uniform corrosion monitoring. This study explores its potential for pitting corrosion monitoring. Specifically, two EMI-based sensor designs were proposed, namely the cylinder and the tube structures. Finite element models were developed to analyze the influence of the pit’s location, morphology parameters, as well as the random distribution of multiple pits, on the conductance peak frequency of sensors. The computer numerical controlled processes were employed to create random pits on sensors. Experimental results revealed that different distributions of pits correspond to distinct conductance peak frequencies, even with the same mass loss. Additionally, the tubular sensor exhibited reduced sensitivity to pits distribution compared to the cylindrical sensor. This is beneficial for accurately predicting mass loss induced by random pitting. This paper enhances the capability of EMI-based sensors for quantitatively monitoring pitting corrosion by focusing on structural design aspects.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.