Abstract
Aligned photoelectrodes have been intensively investigated due to their prominent electron dynamics, but their device performance has been limited by their small surface area. Here, we synthesized vertically aligned TiO2 nanoarchitectures with large internal surface areas and open channels of pores via pulsed laser deposition (PLD) and investigated the effects of the deposition conditions and the postannealing on the formation and properties of nanoarchitecture photoelectrodes for dye-sensitized solar cells. Increasing the oxygen working pressure increases the porosity of the TiO2 film and decreases the amount of deposited materials resulting in an optimized oxygen working pressure of 100 mTorr. The as-deposited films were amorphous and crystallized to the pure anatase phase after annealing at 350 °C or higher. Annealing at higher temperatures resulted in larger grain sizes and larger electron diffusion coefficients. As a result of the compromise between the surface area and crystallinity (or diffusion co...
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have