Abstract

Two different types of Ho2O3 powders (showing a much different morphology) were added to MgB2 in the ex-situ Spark Plasma Sintering (SPS). In the 5–25 K range, the first Ho2O3 powder type does not significantly suppress the critical current density Jc at low magnetic fields and the second one enhances it at high fields, while their mixture simultaneously controls Jc at both small and high magnetic fields so that the decrease is small at low fields and there is a notable enhancement at high fields when compared to pristine sample. The control of Jc(H) is discussed versus specific characteristics of the raw powders, the resulting microstructure of the added SPS-ed samples and pinning details from magnetic relaxation measurements.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.