Abstract
Lead titanate doped with niobium forms solid solutions of the type Pb 1− x/2 (Ti 1− x Nb x )O 3 where x = 0.02 and 0.05. The ferroelectric Curie temperature of these solid solutions is around 465°C, compared to 490°C for PbTiO 3 at the cubic-tetragonal phase change. The lattice distortions at and below the Curie temperature generate internal stresses, leading to microcraking. The microcracking in lead titanate ceramics is detected by acoustic emission methods as a function of heating to and cooling from various temperatures upto 800°C. From this study it is concluded that microcracking is primarily triggered by the sudden lattice parameter changes at the Curie temperature on cooling and that it is enhanced by the anisotropic thermal expansion below the transition. The healing of microcracks is a gradual process and escapes direct detection by the acoustic emission methods. An indication of the recombination of microcracks on heating has been obtained by the total number of acoustic emission counts in samples cooled from various temperatures and also from fixed temperatures after different periods.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.