Marmatite is an important resource of zinc, which exist in forms of high iron and high indium. In order to recycle the valuable metal from these ores, the testwork of simultaneous leaching on neutral residue mixed with zinc concentrate of high iron and high indium has been conducted. The primary objectives are to leach the zinc and indium remaining in the neutral leach residue as ferrite using acid, and to reduce the ferric iron in solution to the ferrous by zinc concentrate, thereby extracting the zinc and indium in the zinc concentrate. The results indicated that in the following conditions, mass ratio of neutral residue to zinc concentrate of 1:0.25, particle size of 74–58 µm, initial sulfuric acid concentration of 150 g/L, liquid to solid ratio of 8 L/kg, temperature of 90°C, reaction time of 4h, the leaching efficiency of zinc and indium were over 95%, nearly 90% Fe was Ferrous in the leaching solution. This process effectively extracted zinc and indium and converted Fe3+ into Fe2+ in solution, and simplified the traditional process of reduction after leaching.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.