Abstract

<001> textured Pb(Ni1/3Nb2/3)O3-PbZrO3-PbTiO3 (PNN-PZT) ceramics were prepared by templated grain growth (TGG) technique using 0.36PNN-xPZ-(0.64-x)PT (x = 0.23, 0.25 and 0.27) powder matrix. Optimum template content was derived to achieve the best electromechanical properties of textured ceramics. The piezoelectric coefficient d33 = 1165 pC/N, Curie temperature TC = 197 °C, longitudinal mode electromechanical coupling factor k33 = 0.86 and a very large effective piezoelectric strain coefficient d33* = 2041 pm/V were simultaneously achieved at the morphotropic phase boundary (MPB) composition (x = 0.25) with 3 vol.% BaTiO3 (BT) templates. Domain structures of textured ceramics were analyzed in detail to reveal the origin of these high piezoelectric and electromechanical properties.