Abstract
The automatic texture enhancement of metal fractographic SEM images is an important part of the metal failure analysis. In this paper, we present a texture enhancement method based on Gaussian high-pass filtering. We find the new method have more clear and useful than other approach in fractographic image. Experimental results show that the texture enhanced images can be classified easily in metal failure analysis process.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: DEStech Transactions on Engineering and Technology Research
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.