Abstract

Three dimensional (3D) metal structures such as nickel (Ni) and copper (Cu) frames have long been regarded as a good host for lithium (Li) metal. However, Li deposition on different metals often causes obvious over-potential, affecting the electrode performance in lithium metal batteries. Here, a Ni-N-O interface was created by surface nitridation to the Ni micro-particles, which were made into 3D current collectors. The directly grown Ni3N created a thin and lithiophilic layer containing dense Li nucleation sites. The homogeneous distribution of amorphous Ni3N and NiO at the interface allowed for a fast transfer of both electrons and ions, and thus facilitated smooth and even plating/stripping of lithium. High cycling stability and rate capability were simultaneously achieved. The 3D Li@N-Ni anode exhibited an extremely low voltage hysteresis of ∼10 mV over 850 h in a symmetric cell. The full battery paired with LiFePO4 achieved steady cycling at 5C for 1500 cycles, with coulombic efficiency constantly higher than 99.2% and an average capacity loss of 0.027 mA h g-1 per cycle, demonstrating a rational strategy for the design and fabrication of efficient lithium anodes for practical applications.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.