AbstractThe experimental study has been done to investigate the through thickness residual stress variation in P91/SS304H welds joint. The gas tungsten arc welding (GTAW) has been performed for joining of the dissimilar metal using the Ni-based ERNiCrMo-3 filler. The residual stress measurement was performed in the weld metal, SS304H HAZ and P92 HAZ. The results showed a considerable deviation in residual stresses along the thickness and in the transverse direction of the weldments. The PWHT showed a significant effect on magnitude and nature of the transverse and longitudinal residual stress for both weld metal and HAZ.KeywordsP91SS304HIN625Residual stressWelding

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.