Abstract

Dual-phase steels containing 0.34 – 2.26 wt.% Si are studied after quenching from the intercritical temperature range. The critical temperatures Ac1 and Ac3 of the steels are determined. The effect of silicon and of the time of holding at 740 – 810°C on the volume fraction of austenite and on the coefficient of silicon distribution between austenite and ferrite is considered.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.