Abstract

Abstract The durability of environment-friendly concrete containing two types of waste material is investigated. Glass powder and microsilica with high silica content were selected to compare their effects on the durability of self-consolidating concrete (SCC) and ordinary concrete with the same packing density in the acidic medium. Experimental results show that microsilica and glass powder do not contribute to concrete corrosion reduction and the most important variable would be superplasticizer content. According to this result, ordinary concretes with lower superplasticizer content show better performance in HCl medium than SCCs. For a quantitative analysis and even to elicit the optimum values for minimum corrosion from the experimental results, an artificial neural network (ANN) and particle swarm optimization (PSO) were used. The minimum mass-loss was related to 15.68% for the volume of permeable pores and the optimum value for compressive strength would be in the range of 32–34 MPa.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.