Abstract

The linear and parabolic oxidation rate constants and activation energies for SiC fibers available in the literature are reviewed for the first time. Oxidation experiments are also conducted with Hi‐Nicalon SiC fibers over 700–1 300 °C in dry O2 with thermogravimetric analysis. Linear oxidation kinetics are observed from 700 to 800 °C and parabolic kinetics are observed from 900 to 1 300 °C. The linear and parabolic oxidation rate constant activation energies are determined to be 83 and 108 kJ mol−1, respectively. These kinetic results are compared with the literature values. Differences in oxidation behavior are assessed as a function of fiber composition.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.