Abstract
Modelling of intergranular stress corrosion cracking (SCC) in pipelines is an important field of study as predictive techniques are integral to pipeline integrity and management. An inclination of the SCC propagation direction has been observed for some pipelines, which is not predictable using existing models as they assume perpendicular crack growth. A review has been conducted to identify the applicable techniques from existing models, as well as the gaps in current knowledge. Existing work in crack growth rates, stress formulations and microstructural representations are reviewed. Mechanical dependency of the electrochemical response is identified as a gap and proposed for inclusion in a model alongside the other areas reviewed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.