Abstract

ObjectiveTo evaluate the durability of a glass ionomer restorative material in Class I and Class II cavities during 10 years compared with a micro filled composite resin. MethodsFifty-nine participants (mean age 24 years) received 140 (80 Class I and 60 Class II) glass ionomer (GI) or composite resin (CR) restorations. Evaluation was performed with slightly modified USPHS criteria at baseline, and yearly during the 10 years. Data were analyzed with Cohran's Q and McNemar's tests. ResultsFifty-one patients and 124 restorations (61 GI / 38 Class I - 23 Class II, 63 CR / 38 Class I, 25 Class II) were evaluated after 10 years. The recall rate was 86.4%. The overall clinical recall rate of restorations was 88.6%. The success rate of Class I and II restorations were calculated as 100% for both materials. The cumulative failure rate (CRF) of all Cl I and Cl II GI restorations was 3.17% in total, but CFR was 8 % for Cl II GI restorations. A significant difference was observed between the marginal discoloration scores of restorations at 10 years (p = 0.022). No significant difference was seen between two restorative materials in terms of marginal adaptation (p > 0.05). A significant change was seen in color match of GI restorations at 10 years (p < 0.05). No significant change was found for the anatomical form, secondary caries, postoperative sensitivity, surface texture, and retention for either restorative material (p > 0.05). ConclusionsBoth tested restorative materials showed an acceptable success rate in the restoration of Class I and Class II cavities during the 10-year follow up.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call