Abstract
Lithium (Li) metal is the ultimate negative electrode due to its high theoretical specific capacity and low negative electrochemical potential. However, the handling of lithium metal imposes safety concerns in transportation and production due to its reactive nature. Recently, anode-free lithium metal batteries (AFLMBs) have drawn much attention because of several of their advantages, including higher energy density, lower cost, and fewer safety concerns during cell production compared to LMBs. Pushing the reversible Coulombic efficiency (CE) of AFLMBs up to 99.98% is key to achieving their 80% capacity retention over more than 1000 cycles. However, interfacial irreversible phenomena such as electrolyte decomposition reactions on both electrodes, dead Li formation, and Li dendrite formation result in poor capacity retention and short circuits in LMBs and AFLMBs. Therefore, it is of great importance and scientific interest to explore those interfacial irreversible phenomena to improve the cell's cycle life. Although significant contributions toward mitigating electrolyte decomposition, dead lithium, and dendritic lithium formation have been reported at the lithium anode, real irreversible phenomena are usually hidden or difficult to discover due to excess lithium employed in LMBs and simultaneous events taking place in both electrodes or at the interfaces.An integrated protocol is suggested to include Li||Cu, cathode||Li, and cathode||Cu configurations to provide overall quantification and determination of various sources of irreversible Coulombic efficiency (irr-CE) in AFLMBs and LMBs. Combining Li||Cu, cathode||Li, and cathode||Cu configurations is essential for separating the root sources of the capacity loss and irr-CE in LMBs and AFLMBs. Remarkably, integrating an anode-free cell with various analytical techniques can serve as a powerful protocol to decouple and quantify those interfacial irreversible phenomena according to our recent reports.In this Account, we focus on the protocol based on an anode-free cell combined with various analytical methods to investigate interfacial irreversible phenomena. Complementary advanced tools such as transmission X-ray microscopy (visualizing Li plating/stripping mechanism), nuclear magnetic resonance spectroscopy (quantifying dead lithium), and gas chromatography-mass spectroscopy (decoupling interfacial reactions) were employed to extract the intrinsic reasons and sources of individual irreversible reactions in LMBs and AFLMBs. Quantitative evaluation of nucleation and growth of Li metal deposition are addressed, along with solid electrolyte interphase (SEI) fracture, visualization of lithium dendrite growth, decoupling of oxidative and reductive electrolyte decomposition mechanisms, and irreversible efficiency (i.e., dead Li and SEI formation) to reveal the intrinsic causes of individual irr-CE in AFLMBs. Meanwhile, an anode-free protocol can also be utilized as a powerful and multifunctional tool to develop electrolyte formulations or artificial layers for LMBs and AFLMBs. Therefore, we also suggest that the anode-free configurations with significant irreversible phenomena can effectively screen and develop new electrolytes. Finally, the concepts of the protocol with an anode-free cell combined with various advanced analytical tools can be extended to provide an in-depth understanding of other metal batteries and solid-state anode-free metal batteries.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.