Abstract

Phosphonic acid functionalization of gellan gum and chitosan biopolymers was successfully performed. In the first step, the sorption was investigated using La(III) ions before testing for the recovery of rare earth elements (REEs) from pretreated industrial acidic leachate. The sorbent was characterized by Fourier-transform infrared (FTIR), scanning electron microscopy with energy dispersive X-ray analysis (SEM-EDX), thermogravimetric analysis (TGA), Brunauer–Emmett–Teller (BET), and pH of zero charge (pHPZC) determination. FTIR and EDX results show efficient grafting of phosphoryl groups. The sorption was determined for the crude materials before functionalization (PGEG) and after phosphorylation (TBP-PGEG). More efficient sorption was seen for phosphorylated sorbent than for the crude composite. The sorption capacity is 0.226 mmol La g−1 for the PGEG while the value is 0.78 mmol La g−1 for the TBP-PGEG. We infer that phosphonate groups participate in the sorption. The most effective sorption is at pH = 4. The kinetic behavior was described using pseudo first-order equations (PFORE), pseudo second-order equations (PSORE), and resistance to intraparticle diffusion (RIDE). The sorption isotherms can be better represented by Langmuir and Sips equations than by the Freundlich equation. The sorbent shows high stability performance during reuse cycles with a limit on the decrease in the sorption performances and stability in the desorption performances. We have thus developed a good tool for the recovery of REEs with a selectivity higher than that of the non-functionalized components.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call