In this study, we produced Cadmium selenide (CdSe) crystalline thin film on commercial glass substrates via chemical bath deposition. Transmittance, absorbance, refractive index and optical bandgap of thin films were examined by UV/vis spectrum. XRD revealed a hexagonal form. The pH level of the baths in which CdSe thin films were deposited varied and optical and structural properties of the resulting thin films were analyzed. SEM analysis was used for surface analysis. Some features of the films were supposed to change with pH and these properties were investigated by testing different pH levels, which were 8, 9, 10 and 11. The variation of the optical bandgap changed between 1.60 and 1.75[Formula: see text]eV, according to the pH of deposition bath. Film thickness varied from 60[Formula: see text]nm to 93[Formula: see text]nm, with the variation of deposition bath’s pH. Moreover, it has been found that refractive index values were also changed with film thickness; these were calculated as 2.28, 2.19, 2.22 and 2.36 for 93.27, 60.97, 61.09 and 60.18[Formula: see text]nm, respectively. Dielectric constant also varied with refractive index, taking values 0.85, 0.75, 0.78, 0.93 for refractive indexes 2.28, 2.19, 2.22 and 2.36, respectively.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.