In a previous published work, the Ti-6Al-4V alloy were functionalized by using plasma enhanced chemical vapour deposition (PECVD) process in order to obtain hydrogenated amorphous carbon (a:C-H) on the biomaterial's surface. At the time, we noticed the functionalized surface contributed to the advance of using Ti-6Al-4V in biomedical implants applications as well as in the adding of intrinsic properties as demonstrated by electrochemical and biological assays. Here, we present new view of a-C:H-coated Ti-6Al-4V alloy, considering the influence of surface free-energy of interaction and understanding how the surface influences the biological response using pre-osteoblastic cells (MC3T3-61). Our results demonstrate, the Ti-6Al-4V containing a:C-H film has less negative value of surface free-energy when compared to the bare material (-22.156 mJ m -2 vs. -60.046 mJ m -2 ), suggesting a tendency toward to a less hydrophobic surface which is extremely important to reduce the inflammatory process, common in orthopedic implants. DOI: http://dx.doi.org/10.17807/orbital.v13i3.1622

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.