Abstract

A good quality Zr:GdTaO4 single crystal with an 8.84 g/cm3 density, higher than the well-known dense scintillator PbWO4, was successfully synthesized by the Czochalski method for the first time. The effective segregation coefficient of Zr in Zr:GdTaO4 is 0.288. The light yield and the energy resolution of Zr:GdTaO4 are approximately the same as GdTaO4. The scintillation decay time of Zr:GdTaO4 contains a fast decay of 9.51 ns, close to the fast scintillator PbWO4, and a slow decay of 755.61 ns, which is much faster than that of GdTaO4 whose fast decay time is 101.82 ns and slow decay time is 3290.52 ns? With Zr4+ doping, the photoluminescence band of GdTaO4 is blueshifted and the traps are shallowed, which may help accelerate the scintillation decay. As far as we know, the Zr:GdTaO4 single crystal is the densest scintillator with a less than 10 ns scintillation decay time, which can be used in electromagnetic calorimeters.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.