Abstract
A novel post-oxidation annealing (POA) process with supercritical N2O (SCN2O) fluid is reported to be highly effective in improving the interface properties of the SiO2/4H–silicon carbide (SiC) (0001) systems. After SCN2O POA, the interface state density reduces to $2.8 \times 10^{{11}}$ eV−1cm−2, which is about 3.5 times lower than that after a traditional high-temperature N2O POA process. Meanwhile, the highest oxide critical electric field shows an increase of 18.19% and the near-interfacial oxide traps is reduced by 69.90% compared with that after N2O POA process. The process temperature is as low as 120 °C. The significantly reduced processing temperature avoids additional defect generation while the supercritical state provides a stronger nitridation effect. SCN2O annealing is a promising candidate for POA process toward high-performance SiC power metal-oxide-semiconductor field effect transistors (MOSFETs).