CdO-Mn3O4 nanocomposite has been prepared by a simple solvothermal method using a domestic microwave oven. Cadmium acetate, manganese acetate and urea were used as the precursors and ethylene glycol as the solvent. The as-prepared sample was annealed for 1 hour in each case at different temperatures, viz. 100, 200 and 300°C. The as-prepared and annealed samples were characterized by X-ray diffraction and scanning electron microscopic analyses. Results indicate that annealing at 300°C is required to get the sample with high phase purity and homogeneity. The present study indicates that the method adopted can be considered as an economical and scalable one to prepare the proposed nanocomposite with reduced size, phase purity and homogeneity.