VO2 powder with superior phase transition performance was prepared by convenient thermolysis method. The results illustrated that VO2 powder show high purity and crystallinity. VO2 particles are transformed from cluster to quasi-sphere with the increase of annealing temperature. The DSC analysis proves that VO2 show superior phase transition performance around 68°C. The phase transition temperature can be reduced to 33.5°C by 1.8at% tungsten doping. The maximum decreasing efficiency of phase transition temperature is about −30K/at% with w=0.4at%. After mixing VO2 powder with acrylic resin, the maximal visible transmission of the composite thin films on glass is 48% and the transmission modulation at 2000nm is 37.3% with phase transition temperature of 66.2°C. Though the phase transition performance is weakened by tungsten doping, the film prepared by 1.3at% tungsten doped VO2 still show superior transmission modulation about 26.4% at 2000nm, which means that it is a potential candidate as smart windows.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.