Abstract

In this study critical pitting temperature (CPT) of two stainless steels is compared using EIS, potentiodynamic and potentiostatic techniques. Two types of stainless steels including DSS2205 and 20Cr–28Ni were chosen. EIS measurements were carried at anodic potential of 600mV/SCE and the results were compared with those of potentiodynamic and potentiostatic polarisations. The results revealed that the CPT of DSS2205 and 20Cr–28Ni was between 45–55°C and 35–45°C in potentiodynamic polarisation, respectively. It was 60 and 55°C for potentiostatic method and between 55–60°C and 45–55°C in EIS method for DSS2205 and 20Cr–28Ni, respectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.