Abstract

The operation of 25 solid oxide cells stacks in steam electrolysis mode over 9000 hours is reported. The stack has been operated at current densities of 0.57 and 0.72 A/cm2, using a 50% steam conversion, in the 750-780°C temperature range. Performance degradation rates of 2.30%/ kh are reported, with some non-homogeneity in the stack repeat units behavior observed. Stack repeat units located at the bottom of the stack feature degradation rates below 2%/kh. The possibility to use the operating temperature as a buffer to counter the performance degradation is highlighted. The stack performance was not affected by incidents that occurred during the test.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.