In this work, atomic layer deposition (ALD) technique has been used as an efficient method to improve the operational stability of quantum dots (QDs) optimized white light emitting diode (WLED), by depositing an alumina layer on the outer surface layer. The luminescent microspheres (LMS) were also employed as QDs composite which had been integrated with yellow phosphors on‐chip packed on blue LED to achieve white light with high color rendering.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.