Abstract

Total and partial outgassing rates after different methods of mechanical and thermal pre-treatments and after different gas exposures of the surface of Inconel 600 specimens have been determined during heating cycles from 20°C up to 520°C. Minimum outgassing rates have been observed from aquablasted surfaces after baking at 700°C for several hours and after gas exposure to N 2. The results of these measurements are important for the treatment of the surface of the first wall of fusion devices using Inconel 600 as a first wall material before the first starting up and during repairs.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.