AbstractPlatinum(Pt) films were sputter-deposited on Si02/Si substrates under the mixed gas atmosphere of Ar and O2. Under certain deposition conditions, the films were oriented such that the (100) direction is normal to the substrate surface. The formation of the (100) texture was affected by the gas pressure and film thickness. After annealing at 650 °C for 1 hour, (100) oriented Pt films with the resistivity of pure Pt were obtained. The annealed Pt films all passed a tape adhesion test and had no defects such as hillocks or pinholes. The experimental results from this work are presented.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.